Metallizing LDPE and Thin PE Films: Outgassing, Wrinkling and Heat Limits
Polyethylene runs on the same metallizers as PET and BOPP, and yet it exposes three limits at once. LDPE melts between 105 °C and 115 °C, its untreated surface energy sits near 31 dyn/cm, and a thin, low-modulus web folds under tension that other films simply ignore. Handle those three limits, and…